PPO 沙伯基础创新塑料(原GE)Sabic LTA1350 无溴阻燃耐老化无填充注塑级聚苯醚优良的电绝缘材料


中文简介:Noryl LTA1350是一种未填充的,可注射成型的等级。为改善长期热老化设计,该树脂还使用非氯化,非溴化FR添加剂,以达到V0 UL94评级。Noryl LTA1350目前有黑色和灰色两种型号,可能是要求电绝缘性能的优良材料。
英文简介:Noryl LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. Noryl LTA1350 is currently available in both black and gray and may be an excellent material candidate for application requiring electrically insulating properties.



SABIC Innovative Plastics NORYL LTA1350 PPE+PS 物性表

物理性能额定值 (公制)额定值 (英制)测试方法
比重1.11 g/cc1.11 g/ccASTM D792
密度1.11 g/cc0.0401 lb/in³ISO 1183
水分吸收0.0600 %0.0600 %23°C / 50% RH; ISO 62
饱和吸水率0.20 %0.20 %ISO 62
线性成型收缩率,Flow0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm

0.0050 - 0.0070 in/in

@Thickness 0.126 in

SABIC Method
熔体流动速率10 g/10 min

@Load 5.00 kg, Temperature 280 °C

10 g/10 min

@Load 11.0 lb, Temperature 536 °F

ASTM D1238
化合物熔体指数10 g/10 min

@Load 5.00 kg, Temperature 280 °C

10 g/10 min

@Load 11.0 lb, Temperature 536 °F

MVR [cm^3/10 min]; ISO 1133
机械性能额定值 (公制)额定值 (英制)测试方法
抗张强度(断裂)60.0 MPa8700 psiType I, 50 mm/min; ASTM D638

80.0 MPa11600 psi50 mm/min; ISO 527
抗张强度(屈服)80.0 MPa11600 psiType I, 50 mm/min; ASTM D638

83.0 MPa12000 psi50 mm/min; ISO 527
伸长率 (断裂)6.0 %6.0 %50 mm/min; ISO 527

18 %18 %Type I, 50 mm/min; ASTM D638
屈服伸长率4.8 %4.8 %Type I, 50 mm/min; ASTM D638

5.0 %5.0 %50 mm/min; ISO 527
拉伸模量2.84 GPa412 ksi1 mm/min; ISO 527

2.85 GPa413 ksi5 mm/min; ASTM D638
弯曲强度118 MPa17100 psi1.3 mm/min, 50 mm span; ASTM D790

131 MPa19000 psi2 mm/min; ISO 178
弯曲模量2.77 GPa402 ksi1.3 mm/min, 50 mm span; ASTM D790

2.91 GPa422 ksi2 mm/min; ISO 178
悬壁梁缺口冲击强度0.900 J/cm1.69 ft-lb/inASTM D256

0.380 J/cm

@Temperature -30.0 °C

0.712 ft-lb/in

@Temperature -22.0 °F

ASTM D256
悬壁梁无缺口冲击强度14.0 J/cm26.2 ft-lb/inASTM D4812
悬壁梁缺口冲击强度4.00 kJ/m²1.90 ft-lb/in²80*10*4; ISO 180/1A

3.00 kJ/m²

@Temperature -30.0 °C

1.43 ft-lb/in²

@Temperature -22.0 °F

80*10*4; ISO 180/1A
悬壁梁无缺口冲击强度35.0 kJ/m²16.7 ft-lb/in²80*10*4; ISO 180/1U

34.0 kJ/m²

@Temperature -30.0 °C

16.2 ft-lb/in²

@Temperature -22.0 °F

80*10*4; ISO 180/1U
简支梁缺口冲击强度0.300 J/cm²1.43 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
落锤总能量17.0 J

@Temperature 23.0 °C

12.5 ft-lb

@Temperature 73.4 °F

ASTM D3763
电气性能额定值 (公制)额定值 (英制)测试方法
体积电阻率3.70e+16 ohm-cm3.70e+16 ohm-cmASTM D257

3.70e+16 ohm-cm3.70e+16 ohm-cmIEC 60093
表面电阻4.20e+14 ohm4.20e+14 ohmASTM D257

4.20e+14 ohm4.20e+14 ohmROA; IEC 60093
介电常数2.7

@Frequency 1.00e+6 Hz

2.7

@Frequency 1.00e+6 Hz

IEC 60250

2.76

@Frequency 1.00e+6 Hz

2.76

@Frequency 1.00e+6 Hz

ASTM D150

2.8

@Frequency 50.0 - 60.0 Hz

2.8

@Frequency 50.0 - 60.0 Hz

IEC 60250

2.87

@Frequency 50.0 - 60.0 Hz

2.87

@Frequency 50.0 - 60.0 Hz

ASTM D150
介电强度18.6 kV/mm

@Thickness 3.20 mm

472 kV/in

@Thickness 0.126 in

in oil; ASTM D149

18.6 kV/mm

@Thickness 3.20 mm

472 kV/in

@Thickness 0.126 in

in oil; IEC 60243-1

30.0 kV/mm

@Thickness 1.50 mm

762 kV/in

@Thickness 0.0591 in

in oil; IEC 60243-1

30.0 kV/mm

@Thickness 1.60 mm

762 kV/in

@Thickness 0.0630 in

in oil; ASTM D149
耗散因数0.0030

@Frequency 1.00e+6 Hz

0.0030

@Frequency 1.00e+6 Hz

ASTM D150

0.0030

@Frequency 1.00e+6 Hz

0.0030

@Frequency 1.00e+6 Hz

IEC 60250

0.025

@Frequency 50.0 - 60.0 Hz

0.025

@Frequency 50.0 - 60.0 Hz

IEC 60250

0.025

@Frequency 50.0 - 60.0 Hz

0.025

@Frequency 50.0 - 60.0 Hz

ASTM D150
相比耐漏电起痕指数(CTI)250 V250 VIEC 60112

250 - 400 V250 - 400 VUL 746A
热丝引燃 (HWI)>= 120 sec>= 120 secUL 746A
高电弧燃烧,HAI0.00 - 15 arcs0.00 - 15 arcsUL 746A
热性能额定值 (公制)额定值 (英制)测试方法
线形热膨胀系数 - 流动83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C

46.1 µin/in-°F

@Temperature -40.0 - 104 °F

ASTM E 831

83.0 µm/m-°C

@Temperature -40.0 - 40.0 °C

46.1 µin/in-°F

@Temperature -40.0 - 104 °F

ISO 11359-2
线性热膨胀系数,横向流动89.0 µm/m-°C

@Temperature -40.0 - 40.0 °C

49.4 µin/in-°F

@Temperature -40.0 - 104 °F

ASTM E 831

89.0 µm/m-°C

@Temperature -40.0 - 40.0 °C

49.4 µin/in-°F

@Temperature -40.0 - 104 °F

ISO 11359-2
Hot Ball Pressure Test<= 135 °C<= 275 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)128 °C

@Thickness 3.20 mm

262 °F

@Thickness 0.126 in

unannealed; ASTM D648

134 °C

@Thickness 6.40 mm

273 °F

@Thickness 0.252 in

unannealed; ASTM D648
载荷下热变形温度(1.8 MPa)115 °C239 °FFlatw 80*10*4 sp=64mm; ISO 75/Af

112 °C

@Thickness 3.20 mm

234 °F

@Thickness 0.126 in

unannealed; ASTM D648

116 °C

@Thickness 6.40 mm

241 °F

@Thickness 0.252 in

unannealed; ASTM D648
维卡软化温度135 °C275 °FRate B/50; ISO 306

137 °C279 °FRate B/120; ISO 306

137 °C279 °FRate B/50; ASTM D1525
UL RTI115 °C239 °FUL 746B
UL RTI,机械冲击120 °C248 °FUL 746B
UL RTI,机械无冲击115 °C239 °FUL 746B
可燃性(UL94)V-0

@Thickness 1.00 mm

V-0

@Thickness 0.0394 in

UL 94 by SABIC-IP
灼热丝试验800 °C1470 °FIEC 60695-2-13

800 °C1470 °FIEC 60695-2-13

800 °C1470 °FIEC 60695-2-13


仓库展示








牌号 Sabic LTA1350
加工级别 注塑级,挤出级
特性级别 阻燃级
用途级别 电子电器部件
品牌 沙伯基础
类型:正牌料 销售方式:品牌经销
产品说明:原厂原包 可卖售地:全国各地
中文名:聚苯醚 产地:上海
产品包装:25KG 外观形状:颗粒
品名:PPO 产品特性:无溴阻燃 耐老化
好货推荐

店铺

收藏

联系

在线咨询
网站也是有底线的
联系电话
  • 18664067255

  • 0769-82690899

联系时请说明
信息来自搜好货网

PPO 沙伯基础创新塑料(原GE)Sabic LTA1350 无溴阻燃耐老化无填充注塑级聚苯醚优良的电绝缘材料

¥ 21.50 ~ ¥ 22.00

规格
价格/数量
无规格

¥21.50

36000千克可售

* 采购数量
* 联系信息
采购明细

询价单发送成功~

电话联系
立即询价
发送询价
完成
图形验证码
点击图片刷新验证码